Poly(lactic acid) (PLA) is a biodegradable plastic with good properties in terms of high tensile strength and high tensile modulus, but the brittleness and low impact strength behavior limit its applications. To enhance the impact strength of PLA, natural rubber (NR) with excellent elastic property should be applied to PLA. However, the polarity difference of these constituents leads the incompatibility resulting in poor mechanical properties of PLA/NR blends. Thus, the chemical modification of NR to increase its polarity is required. This research aimed to synthesize NR-graft-PLA (NR-PLA) as a compatibilizer for PLA/NR blends. There were 2 steps to prepare NR-PLA compatibilizer. Firstly, NR was functionalized by various maleic anhydride (MAH) contents (5-20 phr) to produce NR-MAH having higher polarity than NR. Then, NR-MAH was grafted with PLA via esterification using 4-dimethyaminopyridine (DMAP) as a catalyst. The structural characterization of the NR-MAH and NR-PLA was conducted by FT-IR and ~1H NMR spectrooscopy. This was observed that the increase in the MAH contents increased the amount of grafted MAH in the NR-MAH structure. The higher grafted MAH content induced the greater efficiency for grafting PLA in preparation of NR-PLA. The effects of DMAP, NR/PLA wt ratio and temperature in the esterification step on the grafted PLA were investigated.
机译:聚乳酸(PLA)是一种可生物降解的塑料,在高拉伸强度和高拉伸模量方面具有良好的性能,但其脆性和低冲击强度行为限制了其应用。为了提高PLA的冲击强度,应将具有优异弹性的天然橡胶(NR)应用于PLA。然而,这些成分的极性差异导致不相容性,从而导致PLA / NR共混物的机械性能较差。因此,需要对NR进行化学修饰以增加其极性。这项研究旨在合成NR-PLA(NR-PLA)作为PLA / NR混合物的增容剂。制备NR-PLA增容剂有2个步骤。首先,通过各种含量的马来酸酐(MAH)(5-20​​ phr)对NR进行官能化,以生产极性比NR高的NR-MAH。然后,使用4-二甲基氨基吡啶(DMAP)作为催化剂,通过酯化将NR-MAH接枝到PLA上。 NR-MAH和NR-PLA的结构表征是通过FT-IR和〜1H NMR光谱进行的。观察到,MAH含量的增加增加了NR-MAH结构中的接枝MAH的量。接枝MAH含量越高,则在NR-PLA制备中接枝PLA的效率越高。研究了酯化步骤中DMAP,NR / PLA的重量比和温度对接枝PLA的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号