首页> 外文期刊>Macromolecular symposia >In situ real-time monitoring of a diglycidyl ether of bisphenol a epoxy resin modified with poly(etherimide)/polysulphone blends by simultaneous dielectricear-infrared spectroscopy
【24h】

In situ real-time monitoring of a diglycidyl ether of bisphenol a epoxy resin modified with poly(etherimide)/polysulphone blends by simultaneous dielectricear-infrared spectroscopy

机译:原位实时监测双酚的二缩水甘油醚,通过同时电介质/近红外光谱法对用聚醚酰亚胺/聚砜共混物改性的环氧树脂进行监测

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Simultaneous dielectric and near infrared measurements were performed in "real -time" to follow polymerisation reactions on blends of a diglycidyl ether of bisphenol A (DGEBA) epoxy resin with 4,4'-diaminodiphenylmethane (DDM) hardener and a mixture of polysulphone (PSU) and polyetherimide (PEI) as modifier. All the blends had a 10 wt% of PSU/PEI mixture. The effect of the PEI/PSU ratio in the mixture was studied. Monitoring of the a-relaxation (related to vitrification) was performed by dielectric measurements, while epoxy conversion was followed by near infrared spectroscopy. The effect of the PEI/PSU ratio on this behaviour was studied, as well as that of the curing temperature. Obtained results were compared with that of the blends with neat PSU and PEI as modifiers. [References: 29]
机译:在“实时”下同时进行介电和近红外测量,以跟踪双酚A(DGEBA)环氧树脂的二缩水甘油醚与4,4'-二氨基二苯甲烷(DDM)固化剂和聚砜(PSU)混合物的共混反应)和聚醚酰亚胺(PEI)作为改性剂。所有共混物均具有10重量%的PSU / PEI混合物。研究了混合物中PEI / PSU比的影响。通过介电测量来监测α-松弛(与玻璃化有关),而环氧转化之后是近红外光谱。研究了PEI / PSU比对此行为的影响以及固化温度的影响。将获得的结果与纯PSU和PEI作为改性剂的共混物进行比较。 [参考:29]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号