Effect of accelerated ageing and surface sealing on the permanent deformation of auto-polymerising soft linings

机译:加速老化和表面密封对自聚合软衬永久变形的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Purpose: To compare the effects of different ageing methods on the permanent deformation of two permanent soft liners. Materials and methods: The materials selected were auto-polymerising acrylic resin and silicone-based reliners. Sealer coating was also evaluated. Sixty specimens of each reliner were manufactured (12.7 mm diameter and 19 mm length). Specimens were randomly distributed into 12 groups (n = 10) and submitted to one of the accelerated ageing processes. Permanent deformation tests were conducted with a mechanical device described within the American Dental Association specification number 18 with a compressive load of 750 gf applied for 30 s. All data were submitted for statistical analysis. Mann-Whitney test compared the effect of the surface sealer on each material and the permanent deformation of the materials in the same ageing group (p = 0.05). Kruskal-Wallis and Dunn tests compared all ageing groups of each material (p = 0.05). Results: The silicone-based reliner presented a lower permanent deformation than the acrylic resin-based reliner, regardless of the ageing procedure. The surface sealer coating was effective only for the thermocycled silicone group and the accelerated ageing processes affected only the permanent deformation of the acrylic resin-based material. Conclusion: The silicone-based reliner presented superior elastic properties and the thermocycling was more effective in ageing the materials.
机译:目的:比较不同时效方法对两个永久性软衬套的永久变形的影响。材料和方法:选择的材料是自动聚合丙烯酸树脂和有机硅基衬板。还评估了密封剂涂层。每个衬里制造了60个样品(直径为12.7毫米,长度为19毫米)。将样本随机分为12组(n = 10),并进行加速老化过程之一。用美国牙科协会规格18中描述的机械装置进行永久变形测试,施加​​750 gf的压缩载荷30 s。所有数据均提交进行统计分析。曼恩·惠特尼(Mann-Whitney)测试比较了表面密封剂对每种材料的影响以及同一老化组中材料的永久变形(p = 0.05)。 Kruskal-Wallis和Dunn测试比较了每种材料的所有老化组(p = 0.05)。结果:不论老化程序如何,基于有机硅的衬里都比基于丙烯酸树脂的衬里具有更低的永久变形。表面密封剂涂层仅对热循环的有机硅基团有效,加速的老化过程仅影响丙烯酸树脂基材料的永久变形。结论:有机硅基衬里具有卓越的弹性,热循环对材料的老化更有效。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号