Fabrication and Characterization of Lead Nickel Niobate-Lead Zirconate Titanate Ceramics by Using Two-Stage Sintering Technique

机译:二阶段烧结技术制备铌酸铅铅锆钛酸盐钛酸盐陶瓷及其表征

获取原文
获取原文并翻译 | 示例
           

摘要

In this work, the effects of a two-stage sintering technique on phase formation, mi-crostructure and dielectric properties of perovskite relaxor ferroelectric lead nickel niobate-lead zirconate titanate 0.2PNN-0.8PZT ceramics were investigated by using composition of X-ray diffraction (XRD), scanning electron microscopy (SEM) and dielectric measurements techniques. It was found that the density and grain size values were observed to increase with decreasing the first sintering temperature (T_1) in two-stage sintering method. Under suitable sintering scheme (850/1150℃ for 2 h), highly dense and pure-phase perovskite 0.2PNN-0.8PZT ceramics with maximum dielectric constant of about 22016 at 1 kHz were obtained.
机译:在这项工作中,通过使用X射线衍射的组成,研究了两阶段烧结技术对钙钛矿弛豫铁电体镍铌酸铅锆钛酸钛酸酯0.2PNN-0.8PZT陶瓷的相形成,微观结构和介电性能的影响。 (XRD),扫描电子显微镜(SEM)和介电测量技术。发现在两阶段烧结法中,随着第一烧结温度(T_1)的降低,密度和晶粒度值增加。在合适的烧结方案(850/1150℃,2 h)下,得到了高密度纯相钙钛矿0.2PNN-0.8PZT陶瓷,在1 kHz下的最大介电常数约为22016。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号