Toughening of Poly(L-lactide) with Methyl MQ Silicone Resin

机译:甲基MQ硅树脂增韧聚L-丙交酯

获取原文
获取原文并翻译 | 示例
           

摘要

Poly(L-lactide) (PLLA)/Methyl MQ (M: mono-functional silicon-oxygen unit R_3SiO_(1/2), abbreviated as M; Q: tetra-functional silicon-oxygen unit SiO_2, abbreviated as Q) Silicone Resin (Me-MQ) blends were prepared via a simple solvent evaporation method at various Me-MQ loadings. PLLA is high in strength and modulus, but its applications are limited partly due to its inherent brittleness. It is difficult to keep both toughness and transparency for modified PLLA without compromising its tensile strength and biocompatibility. In this study, we used biocompatible Me-MQ to toughen PLLA at low loadings. The elongation at break of neat PLLA is 7.8%. Tensile test showed that the elongation at break of PLLA blends increased to 67.9% and 217.7% at the loadings of 1 and 2 wt% Me-MQ respectively, with no sacrifice of their strength. UV-vis test showed the light transmittance of the films at the loadings of 1 wt% Me-MQ is almost the same as neat PLLA.
机译:聚(L-丙交酯)(PLLA)/甲基MQ(M:单官能硅氧单元R_3SiO_(1/2),缩写为M; Q:四官能硅氧单元SiO_2,缩写为Q)硅树脂(Me-MQ)共混物是通过简单的溶剂蒸发方法以各种Me-MQ负载量制备的。 PLLA具有很高的强度和模量,但由于其固有的脆性,其应用受到了部分限制。在不损害其抗张强度和生物相容性的情况下,难以同时保持改性PLLA的韧性和透明度。在这项研究中,我们使用了生物相容的Me-MQ在低负荷下增韧PLLA。纯PLLA的断裂伸长率为7.8%。拉伸试验表明,在1和2 wt%的Me-MQ载荷下,PLLA共混物的断裂伸长率分别增加到67.9%和217.7%,而没有牺牲其强度。紫外可见测试表明,在1 wt%Me-MQ的负载下,薄膜的透光率与纯PLLA几乎相同。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号