Effects of powder particle size and binder viscosity on intergranular and intragranular particle size heterogeneity during high shear granulation.

机译:粉末粒度和粘合剂粘度对高剪切造粒过程中粒间和粒内粒度异质性的影响。

获取原文
获取原文并翻译 | 示例
       

摘要

A study was performed in order to elucidate the effects of powder particle size and binder viscosity on intergranular and intragranular particle size heterogeneities. Granules were produced by melt granulation in a high shear mixer from each of four calcium carbonates having mean particle sizes in the range of 5.5-63.1 microm. Each of three polyethylene glycols (PEGs) having viscosities in the range of approximately 40-14,000 mPas were applied as meltable binders. The size distribution of the calcium carbonate particles in three granule size fractions (125-250, 355-500, and 800-1000 microm) was measured after disintegration of the granules. Intragranular particle size heterogeneities were evaluated qualitatively by means of scanning electron microscopy. A preferential growth of the smaller particles was found to give rise to a higher content of small particles in large granules when calcium carbonates with mean particle sizes of 11.7, 34.5, and 63.1 microm were granulated with a binder of low viscosity. The use of a binder of medium or high viscosity leads to a marked reduction of these heterogeneities. A preferential growth of larger particles was seen when calcium carbonates with mean particle sizes of 5.5 and 11.7 microm were granulated with a highly viscous binder. The use of a binder with low or medium viscosity resulted in an increased homogeneity. Intragranular particle size heterogeneities were primarily seen when 5.5 and 11.7 microm calcium carbonate particles were granulated with a highly viscous binder.
机译:为了阐明粉末粒度和粘结剂粘度对粒间和粒内粒度异质性的影响,进行了一项研究。通过在高剪切混合器中熔融造粒,由四种碳酸钙的平均粒径在5.5-63.1微米范围内的每一种来生产颗粒。粘度在大约40-14,000 mPas范围内的三种聚乙二醇(PEG)中的每一种均用作可熔粘合剂。在颗粒崩解后,测量三个颗粒尺寸部分(125-250、355-500和800-1000微米)中碳酸钙颗粒的尺寸分布。通过扫描电子显微镜定性地评价了颗粒内粒度的异质性。当将平均粒径为11.7、34.5和63.1微米的碳酸钙与低粘度的粘合剂制粒时,较小颗粒的优先生长会导致大颗粒中较高含量的较小颗粒。使用中等或高粘度的粘合剂可显着降低这些异质性。当将平均粒径为5.5和11.7微米的碳酸钙与高粘度粘合剂制粒时,可以看到较大颗粒的优先生长。使用低或中粘度的粘合剂导致均匀性增加。当将5.5和11.7微米的碳酸钙颗粒与高粘度的粘合剂制粒时,主要观察到颗粒内粒度的不均匀性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号