Aluminophosphate glasses doped with CdS_xSe_(1-x) have been produced by a wet nonconventional method that provides a better homogeneity of the glass matrix. The glass samples belong to the oxide systems:Li_2O-BaO-Al_2O_3-La_2O_3-SiO_2-P_2O_5andLi_2O-Na_2O-BaO-Al_2O_3- La_2O_3-SiO_2-P_2O_5. The band gaps of the doped samples were determined by UV- VIS-NIR transmission spectro-scopy, using the dependence of the absorption coefficient on photon energy. Structural investigations on semicon-ductor doped glasses were performed by infrared absorp-tion and Raman spectroscopy. Infrared absorption spectra revealed structural units of the phosphate glass matrix. Raman spectra obtained by excitation with 458 and 514 nm revealed CdS_(0.696)Se_(0.304)peaks and by excita-tion with 325 nm, revealed the phosphate matrix bonds. Transmission electron microscopy, selected area electron diffraction (SAED) and fluorescence spectroscopy were used to investigate the semiconductor doped glasses. SAED patterns allowed the calculation of the composition and consequently the band gap of the CdSSe crys-tallites embedded in the glass matrix. A strong CdSSe fluorescence was observed, indicating well ordered crys-tallites with a molar fraction of S and Se close to 0.5 as intended.
机译:掺杂有CdS_xSe_(1-x)的磷酸铝玻璃是通过湿非常规方法生产的,该方法可提供更好的玻璃基质均匀性。玻璃样品属于以下氧化物体系:Li_2O-BaO-Al_2O_3-La_2O_3-SiO_2-P_2O_5和Li_2O-Na_2O-BaO-Al_2O_3-La_2O_3-SiO_2-P_2O_5。利用吸收系数对光子能量的依赖性,通过UV-VIS-NIR透射光谱法确定掺杂样品的带隙。半导体掺杂玻璃的结构研究是通过红外吸收和拉曼光谱进行的。红外吸收光谱揭示了磷酸盐玻璃基质的结构单元。通过在458和514 nm处激发而获得的拉曼光谱显示出CdS_(0.696)Se_(0.304)峰,并且通过在325 nm处被激发而显示出磷酸盐基体键。透射电子显微镜,选择区域电子衍射(SAED)和荧光光谱用于研究掺杂半导体的玻璃。 SAED图案可以计算组成,并因此可以计算嵌入玻璃基质中的CdSSe晶状体的带隙。观察到强烈的CdSSe荧光,表明S和Se的摩尔分数接近预期的0.5良好的有序晶体。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号