In situ Raman microscopy during discharge of a high capacity silicon-carbon composite Li-ion battery negative electrode

机译:高容量硅碳复合锂离子电池负极放电过程中的原位拉曼显微镜

获取原文
获取原文并翻译 | 示例

摘要

In situ Raman microscopy study has been performed in order to characterize the surface of the Si/C composite anode and also to monitor the alloying/dealloying behavior of Si/C with Li ion during electrochemical discharging/charging processes at a microscopic level. This study shows that the Si particles are covered by graphite and hard carbon, with demonstration of further evidence of amorphisation of silicon and presence of mixed phases of Li-Si. (C) 2008 Elsevier B.V. All rights reserved.
机译:为了表征Si / C复合阳极的表面特性,并在微观水平上监测电化学放电/充电过程中Si / C与Li离子的合金化/脱合金行为,已进行了原位拉曼显微镜研究。这项研究表明,硅颗粒被石墨和硬碳覆盖,并进一步证明了硅的非晶化和锂硅混合相的存在。 (C)2008 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号