As the standard toxicity characteristic leaching procedure (TCLP) can not exhaust the acid neutralizing capacity of the cement rotary kiln co-processing solid wastes products which is particularly important for the assessment of the leaching concentrations of heavy metals. A modified TCLP was proposed. The extent of leaching of heavy metals is low using the TCLP and the leaching performance of the different metals can not be differentiated. Using the modified TCLP, however, Zn leaching was negligible during the first 180 h and then sharply increased (2.86 +/- A 0.18 to 3.54 +/- A 0.26 mg/L) as the acidity increased (pH 6.0). Thus, Zn leaching is enhanced using the modified TCLP. While Pb leached readily during the first 126 h and then leachate concentrations decreased to below the analytical detection limit. To conclude, this modified TCLP is a more suitable method for these cement rotary kiln co-processing products.
机译:由于标准的毒性特征浸出程序(TCLP)不能耗尽水泥回转窑共处理固体废物产品的酸中和能力,这对于评估重金属的浸出浓度尤为重要。提出了修改后的TCLP。使用TCLP时,重金属的浸出程度较低,并且无法区分不同金属的浸出性能。但是,使用改良的TCLP,锌的浸出在最初的180小时内可以忽略不计,然后随着酸度的增加(pH <6.0)急剧增加(2.86 +/- A 0.18至3.54 +/- A 0.26 mg / L)。因此,使用改进的TCLP可以增强锌的浸出。在开始的126小时内,铅很容易浸出,然后沥出液的浓度降至分析检测极限以下。总而言之,这种改进的TCLP是更适合这些水泥回转窑共处理产品的方法。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号