In this work, we prepared a Pt/TiO2 electrocatalyst for methanol electrooxidation. The Pt nanoparticles were loaded on the alkali-treated nanoporous TiO2 by a convenient deposition method. The morphology of the nanoporous TiO2 was depended on the alkali treatment time. After 15-min alkali treatment, the flocculent-liked nanostructure was formed, and the specific surface area of the material was the largest. The amounts as well as the size and distribution of Pt nanoparticles were controlled by loading times. The catalytic activities of the catalysts toward methanol electrooxidation were tested in the alkaline condition. The alkali treatment time and chemical loading time were the key factors that influenced the catalytic activities. The optimal catalytic activity was achieved when the loading time was six.
机译:在这项工作中,我们制备了用于甲醇电氧化的Pt / TiO2电催化剂。通过方便的沉积方法将Pt纳米颗粒负载在碱处理的纳米多孔TiO2上。纳米多孔TiO 2的形态取决于碱处理时间。经过15分钟的碱处理,形成了絮状纳米结构,材料的比表面积最大。 Pt纳米粒子的数量,大小和分布是通过加载时间控制的。在碱性条件下测试了催化剂对甲醇电氧化的催化活性。碱处理时间和化学负载时间是影响催化活性的关键因素。当加载时间为六时,获得了最佳的催化活性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号