Hydrogen cycling induced diffraction peak broadening in C14 and C15 Laves phases

机译:氢循环在C14和C15 Laves相中引起的衍射峰展宽

获取原文
获取原文并翻译 | 示例
       

摘要

The diffraction peak broadening induced by hydrogen absorption-desorption cycling has been analyzed in four different Laves phase compounds with the C14 and C15 structures. The broadening is due to strain most probably originating from dislocations generated at the interface between the alpha and beta hydride phases in connection with the cell volume difference between the two phases. It has been shown that it is strongly compound dependent. In the case of the C14 structure, the broadening is large and isotropic, and the latter can be related to the isotropy of the elastic constants of the metallic phase. The broadening is less for the compounds with the C15 structure, which can be related to a possibly softer lattice. Better ageing properties after long-term cycling are predicted for this crystal structure. (c) 2005 Elsevier Inc. All rights reserved.
机译:在四种具有C14和C15结构的Laves相化合物中,分析了由氢吸收-解吸循环引起的衍射峰展宽。变宽是由于应变最可能源自与两个相之间的细胞体积差异有关的α和β氢化物相之间的界面处产生的位错。已经表明它是强烈依赖化合物的。在C14结构的情况下,展宽大且各向同性,而后者可能与金属相的弹性常数的各向同性有关。具有C15结构的化合物的加宽幅度较小,这可能与可能较软的晶格有关。对于该晶体结构,经过长期循环后,其老化性能更好。 (c)2005 Elsevier Inc.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号