Pure molybdenum was sintered with SPS under various temperatures, external pressures and heating rates. The microstructure of the specimens representing the different sintering conditions was investi-gated by classical metallographic methods. The relative density, the microhardness and the chord length distribution were measured. Linear shrinkage, depending on time or temperature, was calculated from piston travel, which was recorded during sintering process. These results show that the main part of con-solidation takes place during fast heating up. The densification behaviour is controlled mainly by sinter-ing temperatures and applied pressure. The molybdenum powder was successfully consolidated by SPS in very short times. A relative density of 95% was reached by sintering temperatures of 1600 °C and external pressure of 67 MPa.
机译:在各种温度,外部压力和加热速率下,将纯钼与SPS一起烧结。用经典金相方法研究了代表不同烧结条件的试样的显微组织。测量相对密度,显微硬度和弦长分布。根据时间或温度,根据活塞的行程计算出线性收缩率,并在烧结过程中记录下来。这些结果表明,固结的主要部分发生在快速加热期间。致密化行为主要由烧结温度和施加压力控制。 SPS在很短的时间内成功地将钼粉固结。烧结温度为1600°C,外部压力为67 MPa,相对密度为95%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号