摘要

Cracking occurs often at "near-seam zone" in the girth weld joint of an X70 pipeline in tensile test, which is considered unacceptable for strain-based design pipelines according to some current standards. The tensile strain capacity of girth weld joints for X70 pipelines with "near-seam zone" cracks has thus been studied via the approach of crack driving force and fracture resistance curve. The high strain capacity has been demonstrated by resistance curve tangency approach and curved wide plate test. The results prove that the girth weld joint has considerable fracture resistance and is thus of high strain capacity. (C) 2016 Elsevier Ltd. All rights reserved.
机译:在拉伸试验中,裂纹通常发生在X70管道的环缝焊接接头的“近接缝区域”,根据一些现行标准,这对于基于应变的设计管道是不可接受的。因此,通过裂纹驱动力和抗断裂强度曲线研究了具有“近缝区”裂纹的X70管道的环缝焊接接头的拉伸应变能力。高应变能力已通过电阻曲线相切法和弯曲宽板试验证明。结果证明环焊缝具有相当大的抗断裂性,因此具有高应变能力。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号