The cone and plate method is used to quantify the effect of shearing rate, shearing time, and molten alloy temperature on the rheological properties of strontium modified and unmodified near eutectic Al-Si alloys. It is found that in the temperature range 583℃ (1,08I°F) to 598℃ (1,108°F) at relatively low shear rates, these alloys behave as Non-Newtonian fluids. In addition, they exhibit shear-thinning, and at all the shear rates tested, the viscosity of the Sr-modified alloys is higher than that of the unmodified alloys.
机译:锥板法用于量化剪切速率,剪切时间和熔融合金温度对锶改性和未改性的近共晶Al-Si合金流变性能的影响。发现在相对较低的剪切速率下,在583℃(1,08I°F)至598℃(1,108°F)的温度范围内,这些合金的行为类似于非牛顿流体。另外,它们表现出剪切稀化,并且在所有测试的剪切速率下,Sr改性合金的粘度均高于未改性合金的粘度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号