The cohesive zone parameters (separation energy and cohesive strength) and the crack tip triaxialities are compared between a compact tension (CT) and a double edge notched tension (DENT) specimen with smooth side-surfaces. The material is a pressure vessel steel 20MnMoNi55. The cohesive zone parameters are determined by fitting the simulated crack extensions near the mid-section to the experimental data. The purpose of the study is to understand the relationship between the cohesive zone parameters and the crack tip stress triaxiality. The results show that for the same cohesive zone parameters the crack tip triaxiality near the midsection is lower in DENT specimens than in CT specimens. When the separation energy is set constant for CT and DENT specimens, the cohesive strength for the DENT specimens should be significantly lower than that for the CT specimens in order to make the simulated crack extensions near the midsection fit to the experimental data. Near the midsection, the cohesive strength and crack tip triaxiality influence each other: the specimen with a higher stress triaxiality has a higher cohesive strength; an increase of cohesive strength results in an increase of the crack tip triaxiality.
机译:比较了具有紧密侧面的紧凑张力(CT)和双边缘缺口张力(DENT)试样的内聚力区域参数(分离能和内聚强度)和裂纹尖端的三轴性。该材料是压力容器钢20MnMoNi55。通过将中段附近的模拟裂纹扩展与实验数据拟合,可以确定粘性区域参数。研究的目的是了解内聚区参数与裂纹尖端应力三轴性之间的关系。结果表明,对于相同的粘结带参数,DENT样品中段附近的裂纹尖端三轴性比CT样品低。当将CT和DENT试样的分离能设置为常数时,DENT试样的内聚强度应显着低于CT试样的内聚强度,以使中部附近的模拟裂纹扩展符合实验数据。在中部附近,内聚强度和裂纹尖端的三轴性相互影响:应力三轴性较高的试样具有较高的内聚强度;内聚强度的增加导致裂纹尖端三轴性的增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号