TiO2 coating was deposited on a pure titanium substrate using a micro-arc oxidation (MAO) process in an electrolyte solution with the NaAlO2 addition varying from 0 to 0. 4 g/l. With increasing NaAlO2 concentration, the working voltage could effectively increase and promoted the growth rate of MAO coatings on pure titanium. The X-ray diffraction (XRD) results indicated that MAO coatings mainly consisted of TiO2(B), rutile, and anatase. The surfaces of the MAO coatings which were formed on pure titanium in the electrolyte without NaAlO2 mainly consisted of micro-pores. The number of the sintered disc and the discharge channel diameter increased with increasing NaAlO2 concentration. The corrosion rates of MAO coatings decreased at the first and then increased. (C) 2016 Elsevier B.V. All rights reserved.
机译:TiO2涂层在电解质溶液中使用微弧氧化(毛)工艺沉积在纯钛基板上,NaAlO2添加量从0到0不等。4 克/升。随着NaAlO2浓度的增加,工作电压可以有效提高和促进纯钛上毛涂层的生长速度。X射线衍射(XRD)结果表明,毛涂层主要由TiO2(B)、金红石和锐钛矿组成。在不含NaAlO2的电解液中,纯钛上形成的毛涂层表面主要由微孔组成。烧结盘数和放电通道直径随NaAlO2浓度的增加而增大。毛涂层的腐蚀速率先降低后增加。(c) 2016 Elsevier B.V.保留所有权利。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号