The composition and structure of solid char residues after thermal degradation of polystyrene, PVC and polyamide. Part I

机译:The composition and structure of solid char residues after thermal degradation of polystyrene, PVC and polyamide. Part I

获取原文
       

摘要

AbstractThe study of char residues after thermal degradation of synthetic polymers, especially the identification of their morphology, structure and chemical composition is presented in this paper. Special attention was focused on the polystyrene, PVC and polyamide char residues. By means of microscopy in reflected light and reflected polarized light the manifestations of optical anisotropy were observed. X‐ray analysis was used for the examination of the microstructure of PVC char residues carbonized at temperatures above 1000°C. For PVC char residues the electric resistivity was determined. The results have proved the close connection between the structure and properties of char residues and the intensity and course of thermal degradation of polyme

著录项

  • 来源
    《fire and materials》 |1985年第3期|145-149|共页
  • 作者

    P. Ševěček; P. Dvořák;

  • 作者单位
  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 英语
  • 中图分类
  • 关键词

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号