Characterization of bismuth vanadate (BiVO4) nanoparticle prepared by solvothermal method

机译:溶剂热法制备钒酸铋(BiVO4)纳米粒子的表征

获取原文
获取原文并翻译 | 示例
           

摘要

Bismuth vanadate (BiVO4) nanoparticle was prepared by solvothermal method. The starting precursors were used as bismuth nitrate pentahydrate (Bi(NO3)(3)center dot 5H(2)O), ammonium metavanadate (NH4VO3) and absolute ethanol (C2H5OH). Solution I: Bi(NO3)(3)center dot 5H(2)O was dissolved in 2.0M nitric acid (HNO3) and absolute ethanol (C2H5OH). Solution II: NH4VO3 was dissolved in 2.0M ammonium hydroxide (NH4OH) and absolute ethanol (C2H5OH). The mixed solutions were stirred for 5min and left into Teflon-lined stainless steel autoclave treatment at 200 degrees C for 3 and 5h. The yellow final solution was filtered and dried at 100 degrees C for 24h. All BiVO4 nanoparticle samples were characterized by X-ray diffractometer (XRD), field emission scanning electron microscope (FESEM), energy dispersive X-ray spectrometer (EDXS) and Fourier transform infrared spectrometer (FTIR).
机译:溶剂热法制备了钒酸铋(BiVO4)纳米粒子。起始前体用作五水合硝酸铋(Bi(NO3)(3)中心点5H(2)O),偏钒酸铵(NH4VO3)和无水乙醇(C2H5OH)。溶液I:将Bi(NO3)(3)中心点5H(2)O溶于2.0M硝酸(HNO3)和无水乙醇(C2H5OH)中。溶液II:将NH4VO3溶于2.0M氢氧化铵(NH4OH)和无水乙醇(C2H5OH)中。将混合的溶液搅拌5分钟,并在200℃下放入特氟隆衬里的不锈钢高压釜处理3和5h。将黄色的最终溶液过滤并在100℃下干燥24h。所有BiVO4纳米颗粒样品均通过X射线衍射仪(XRD),场发射扫描电子显微镜(FESEM),能量色散X射线光谱仪(EDXS)和傅里叶变换红外光谱仪(FTIR)进行了表征。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号