AbstractExtrusion experiments on eight polymers in our laboratory and eight additional polymers in other laboratories reveal that solid‐state extrusion and malleability occur in semicrystalline polymers that have a reversible crystalline transition,Tc, and do not occur in crystalline polymers devoid ofTc, The solid‐state extrusion takes place only in the temperature range ofTc≪T展开▼