The sieved coal gangue is used to replace part of the aggregate of the ordinary cement stabilised crushed stone to optimise the mix ratio design. The results of the study show that after optimisation tests, the mass fraction of cement in the coal gangue cement stabilised base material is 6, and the average unconfined compressive strength for 7 days is 5.5 MPa. After 90 days of curing, the specimens prepared according to the optimised gradation have a compressive resilience modulus of 2800 to 3 500 MPa, a splitting strength of 0.688 to 0.763 MPa, and an unconfined compressive strength of about 7 days. 75 of 90 d. Cement-stabilised coal gangue meets the mechanical index requirements of substituting the base course and base course materials.
机译:筛煤矸石用于替代普通水泥稳定碎石的部分骨料,以优化混合比设计。研究结果表明,经过优化试验,煤矸石水泥稳定基材中水泥的质量分数为6%,7 d的平均无侧限抗压强度为5.5 MPa。固化90 d后,根据优化级配制备的试样具有2800至3 500 MPa的抗压回弹性模量,劈裂强度为0.688至0.763 MPa,无侧限抗压强度约为7 d。90 d的75%。水泥稳定煤矸石满足基层和基层材料替代的力学指标要求。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号