A mass of Longquan porcelain shards carved with Guan' or the dragon patterns were unearthed in the early Ming Dynasty layer of the Fengdongyan kiln site at Dayao County. These celadon shards were fired in the Hongwu and Yongle eras of the Ming Dynasty. In order to research the raw materials and firing technology of the imperial porcelain, 85 typical shards were analysed by energy-dispersive X-ray fluorescence (EDXRF). The results indicate that the contents of TiO2 and Fe2O3 in the body vary in the Hongwu and Yongle eras. Compared with Longquan glazes in the Southern Song Dynasty, the average values of K2O, Fe2O3 and TiO2 are higher, but that of CaO is lower in early Ming imperial porcelain glazes. Principal components analysis (PCA) shows that different degrees of elutriation of the same raw materials are the main reason for this difference in the Hongwu and Yongle periods. However, the raw materials of imperial porcelain glazes show no obvious changes and have inherited the earlier tradition. The production and firing technology of imperial porcelain reached a higher level and had not declined in the Early Ming Dynasty.
机译:在大姚县风洞岩窑遗址明朝初层,出土了一大批刻有“关”或“龙”图案的龙泉瓷片。这些青瓷碎片是在明朝的洪武时代和永乐时代发射的。为了研究帝国瓷器的原料和烧制工艺,采用能量色散X射线荧光光谱仪(EDXRF)分析了85种典型的碎片。结果表明,在洪武时代和永乐时代,人体中TiO2和Fe2O3的含量各不相同。与南宋龙泉釉相比,明代早期瓷釉中的K2O,Fe2O3和TiO2平均值较高,而CaO的平均值较低。主成分分析(PCA)表明,在洪武时期和永乐时期,相同原材料的不同淘析程度是造成这种差异的主要原因。但是,帝制瓷釉的原料没有明显变化,并且继承了较早的传统。明代初期,御瓷的生产和烧制技术达到了较高的水平,并没有下降。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号