La2O3/gamma-Al2O3, NiO/gamma-Al2O3 and NiO/La2O3/gamma-Al2O3 samples have been prepared by conventional impregnation, using silica-free gamma-Al2O3 support. The materials have been characterized, as such or after reaction, with XRD, skeletal IR, UV-vis-NIR, XPS and FESEM techniques. The catalytic activity has been evaluated in ethanol decomposition through temperature programmed surface reaction (TPSR); and in ethanol steam reforming (ESR); and in mixed ethanol and phenol steam reforming (EPSR as a model reaction for biomass tar steam reforming) in a continuous flow reactor. Ni on alumina exists as a surface NixAl2O3+x spinel, evident by XRD, skeletal IR and vis spectroscopy measurements. La disperses on alumina in a disordered state. In the ternary system, XPS reveals significant Ni-La interactions. The addition of some lanthanum further increases the activity of Ni/Al2O3 for ESR and EPSR. Fresh unreduced catalysts are conditioned in the feed at temperatures above 973 K. Conditioned catalysts give rise to full conversion of reactants in ESR and EPSR at 873 K and higher temperatures, but are severely deactivated by sulfur. The sudden start of the steam reforming activity at 873 K likely corresponds to the temperature onset for the activation of water by metallic nickel. (C) 2015 Elsevier B.V. All rights reserved.
机译:La2O3 /γ-Al2O3,NiO /γ-Al2O3和NiO / La2O3 /γ-Al2O3样品是使用无二氧化硅的γ-Al2O3载体通过常规浸渍制备的。如此或在反应之后,已使用XRD,骨架IR,UV-vis-NIR,XPS和FESEM技术对材料进行了表征。已通过程序升温表面反应(TPSR)对乙醇分解中的催化活性进行了评估;以及乙醇蒸汽重整(ESR);连续流反应器中的乙醇和苯酚混合蒸汽重整(EPSR作为生物质焦油蒸汽重整的模型反应)。氧化铝上的镍以表面NixAl2O3 + x尖晶石的形式存在,这通过X射线衍射,骨架红外和可见光谱测量可以明显看出。 La以无序状态分散在氧化铝上。在三元系统中,XPS揭示了重要的Ni-La相互作用。某些镧的添加进一步增加了Ni / Al2O3对ESR和EPSR的活性。新鲜的未还原催化剂在进料中在高于973 K的温度下进行调节。经过调节的催化剂可在873 K和更高的温度下使ESR和EPSR中的反应物完全转化,但会因硫而严重失活。蒸汽重整活动在873 K突然开始可能与金属镍活化水的起始温度相对应。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号