The effect of the Pd loading in NiO-MgO solid solution was investigated in oxidative steam reforming of methane under atmospheric and pressurized conditions. The small amounts of Pd addition on Ni0.2Mg0.8O can inhibit the oxidation of Ni species and the mixture can maintain the reforming ability at low W/F conditions under atmospheric pressure, where Ni0.2Mg0.8O catalyst deactivated. In addition, Ni0.2Mg0.8O catalyst improved remarkably, gaining both high activity and excellent stability by the addition of small amounts of Pd under pressurized conditions. The deactivation rate was closely related to the amount of deposited carbon. Characterization results of TEM, TPR, EXAFS and FTIR suggest that Pd-Ni alloy particles are formed on Pd/Ni0.2Mg0.8O catalysts. The Pd-Ni alloy particles with a low ratio of I'd to Ni can play an important role in the high resistance to carbon deposition. (c) 2006 Elsevier B.V. All rights reserved.
机译:在常压和加压条件下,在甲烷的氧化蒸汽重整中,研究了NiO-MgO固溶体中Pd负载的影响。在Ni0.2Mg0.8O上少量添加Pd可以抑制Ni物种的氧化,在低W / F条件下,Ni0.2Mg0.8O催化剂失活后,混合物可以保持重整能力。此外,Ni0.2Mg0.8O催化剂显着改善,通过在加压条件下添加少量Pd可获得高活性和出色的稳定性。失活速率与沉积的碳量密切相关。 TEM,TPR,EXAFS和FTIR的表征结果表明,在Pd / Ni0.2Mg0.8O催化剂上形成Pd-Ni合金颗粒。 Id与Ni的比例低的Pd-Ni合金颗粒可在高抗碳沉积性方面发挥重要作用。 (c)2006 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号