Decomposition of CCl4, CCl2F2 CCIF3, and CF4 was studied in the presence of water vapor over AIPO(4). They began to decompose at about 300, 330, 450, and 550 degrees C, respectively. A good linear relationship between the reactivity of CFCs and the bond dissociation energy of the C-Cl bond suggests that the C-CI bond cleavage is the rate-determining step. The lattice structure of AIPO(4) before reaction was slightly distorted but the environment of Al and P ions became uniform after the reaction, consistent with a slight progress of crystallization of AlPO4. Supporting AlPO4 onto active charcoal is not preferable to the support because of its reactivity to water vapor. ALPO-5 was less active than that AIPO(4) because the inside of the pores of ALPO-5 is hydrophobic and not effective for the CCl2F2 decomposition. Meso-porous AlPO4 showed almost the same activity with AlPO4, but the destruction of the meso-porous structure brought about a loss of activity at 400 degrees C. (C) 2000 Elsevier Science: B.V. All rights reserved. [References: 10]
机译:在AIPO(4)上存在水蒸气的条件下研究了CCl4,CCl2F2 CCIF3和CF4的分解。它们分别在约300、330、450和550摄氏度开始分解。 CFC的反应性与C-Cl键的键解离能之间存在良好的线性关系,这表明C-CI键的裂解是决定速率的步骤。反应前AIPO(4)的晶格结构略有变形,但反应后Al和P离子的环境变得均匀,这与AlPO4的结晶过程略有一致。将AlPO 4负载在活性炭上不是载体,因为它对水蒸气具有反应性。 ALPO-5的活性不如AIPO(4),因为ALPO-5的孔内部是疏水性的,对CCl2F2的分解无效。介孔AlPO4具有与AlPO4几乎相同的活性,但是介孔结构的破坏导致在400摄氏度下失去活性。(C)2000 Elsevier Science:B.V.保留所有权利。 [参考:10]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号