Influences of calcination temperature on the efficiency of CaO promotion over CaO modified Pt/γ-Al2O3 catalyst

机译:煅烧温度对CaO改性Pt /γ-Al2O3催化剂上CaO促进效率的影响

获取原文
获取原文并翻译 | 示例
           

摘要

The cyclohexane dehydrogenation on CaO modified Pt/γ-Al2O3 was investigated-with the aim of understanding the influences of calcination temperature of CaO modified γ-Al2O3 support (Ca/Al) on the efficiency of CaO promotion. The results showed that the catalyst calcined at 600 °C exhibited the worst, while the one calcined at 800 °C showed the best catalytic performance during the variation of Ca/Al calcination temperature from 500 to 900 °C The catalyst pretreated at 800 °C exhibited an excellent hydrogen productivity of up to 4.45 L/(g_(cat) h) and high stability during 80 h continuous investigation of cyclohexane dehydrogenation in the absence of co-feed hydrogen at 300 °C and 8000 h~(-1) space velocity. That was attributed to weaker Pt-Al interaction and higher dispersed Pt, deriving from larger CaO particles. According to XRD spectra of model catalysts and CO2-TPD of Ca-Pt/Al catalysts, the efficiency of CaO promotion depended on the Ca-Al interaction strength and particle size instead of quantity of free CaO particles. The main calcium compound was free CaO in catalysts with low CaO content and low calcination temperature (below 800 °C). Complex CaO with high Ca-Al interaction strength and less CaO properties are formed in Ca900-Pt/AI catalyst.
机译:为了了解CaO改性的γ-Al2O3载体(Ca / Al)的煅烧温度对CaO促进效率的影响,研究了环己烷在CaO改性的Pt /γ-Al2O3上的脱氢反应。结果表明,在Ca / Al煅烧温度从500到900°C的变化范围内,在600°C煅烧的催化剂表现最差,而在800°C煅烧的催化剂表现出最好的催化性能。在300°C和8000 h〜(-1)空间不存在共进料氢的情况下,在不进行共进料氢的情况下连续研究环己烷脱氢的80 h期间,具有高达4.45 L /(g_(cat)h)的优异氢气生产率和高稳定性速度。这是由于较大的CaO颗粒导致Pt-Al相互作用较弱和Pt分散较高。根据模型催化剂的XRD谱图和Ca-Pt / Al催化剂的CO2-TPD,CaO的促进效率取决于Ca-Al的相互作用强度和粒径,而不是游离的CaO颗粒的数量。在低CaO含量和低煅烧温度(低于800°C)的催化剂中,主要的钙化合物是游离CaO。在Ca900-Pt / Al催化剂中形成具有高Ca-Al相互作用强度和较少CaO性能的复合CaO。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号