Hot Corrosion Behavior of YSZ and CaZrO3/YSZ Composite Thermal Barrier Coatings in Contact with 50V(2)O(5)+50Na(2)SO(4) Salts

机译:YSZ和Cazro3 / YSZ复合热阻挡涂层的热腐蚀行为与50V(2)O(5)+ 50NA(2)如(4)盐

获取原文
获取原文并翻译 | 示例
           

摘要

A novel thermal barrier coating system was formulated to resist hot corrosion environments. In this coating system, 5% CaZrO3 was added to conventional yttria-stabilized zirconia (YSZ). The above composite coating system was compared with the standard YSZ system in the presence of a mixture of 50% Na2SO4 and 50% V2O5 at 950 A degrees C. The results demonstrated that the lifetime of the CaZrO3-added composite system in this highly hostile environment was longer compared with the standard YSZ system. This is due to the fact that the preferential reaction of NaVO3 shifted from yttria to calcia, forming CaV2O4 instead of YVO4. The preferential reactions are discussed in terms of free energy changes and acid-base theory of molten salts with ceramic oxides. Furthermore, calculations of lattice distortion also proved that the CaZrO3-added composite system demonstrated less distortion, thus increasing the overall lifetime of the coating system.
机译:研制了一种新型热障涂层系统,以抵抗热腐蚀环境。在该涂层体系中,向传统的钇稳定氧化锆(YSZ)中添加5%的CaZrO3。将上述复合涂层系统与标准YSZ系统在950℃温度下存在50%Na2SO4和50%V2O5的混合物时进行比较。结果表明,与标准YSZ系统相比,添加CaZrO3的复合系统在这种高度恶劣环境中的寿命更长。这是因为NaVO3的优先反应从钇转移到钙,形成CaV2O4而不是YVO4。根据自由能变化和熔融盐与陶瓷氧化物的酸碱理论讨论了优先反应。此外,晶格畸变的计算还证明,添加CaZrO3的复合体系表现出较小的畸变,从而提高了涂层系统的整体寿命。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号