It's worth cleaning - The examination of the female taper could identify a particular cause of trunnionosis at revision 16 years after total hip arthroplasty

机译:值得清洁 - 雌性锥度的检查可以在总髋关节关节造身术后16年内识别修订版的特定原因

获取原文
获取原文并翻译 | 示例
       

摘要

Adverse reaction to metal debris (ARMD) is an issue in metal-on-metal (MoM) total hip replacements (THR). It mainly affects large-head MoM THR, whereas 28-32 mm MoM pairings are associated with low long-term revision rates. However, the bearing surface is not necessarily the only cause of metal debris. This report documents with advanced analysis of the retrievals a particular cause of trunnionosis in late failure of a small diameter MoM THR and illustrates the importance of cleaning of the taper when seating the head in THR. A 65-year-old patient was revised due to ARMD 16 years after small diameter MoM THR. Debridement and exchange of the inlay and the head had been performed through an anterior approach. While the cup and the outer surface of the head were accessible to direct analysis by an optical coordinate measuring machine, the female taper had to be analysed indirectly by measuring an imprint. Wear from the cup and the head was within expected low ranges. The analysis of the female taper identified bone fragments, which contributed to trunnionosis. Failure due to ARMD after MoM THR is not necessarily caused by the bearing, but can be due to trunnionosis. Bone fragments within the taper contact in this case highlight the importance of meticulous cleaning of the taper before seating the head, to avoid trunnionosis.
机译:金属碎片不良反应(ARMD)是金属对金属(MoM)全髋关节置换术(THR)中的一个问题。它主要影响大头MoM THR,而28-32毫米MoM配对与低长期翻修率相关。然而,轴承表面不一定是金属碎屑的唯一原因。本报告记录了小直径MoM THR晚期失效时耳轴病的一个特殊原因,并对回收进行了深入分析,说明了在将头部固定在THR中时清洁锥度的重要性。一名65岁的患者在小直径MoM THR术后16年因ARMD而改型。通过前路进行了清创和嵌体与头部的交换。虽然可以通过光学坐标测量机直接分析罩杯和头部外表面,但必须通过测量印记间接分析内锥。杯子和头部的磨损在预期的低范围内。对女性圆锥的分析确定了导致耳轴病的骨碎片。MoM THR后由于ARMD导致的故障不一定是由轴承引起的,但可能是由于耳轴病。在这种情况下,锥形接触内的骨碎片突出了在固定头部之前仔细清洁锥形的重要性,以避免耳轴病。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号