Wood can be used for the in situ preparation of wood sponge using chemical treatment, which can be employed as absorbent for sewage treatment and exhibits the advantage of low cost, low density, high porosity, and environmental friendliness. Previous researches on wood sponge mainly focused on its various applications, while the influence rule and mechanism of treatment conditions such as pH and concentration of NaClO2 solution, as well as concentration of NaOH solution have not been fully understood. This challenge limits the manufacturing efficiency and further application of wood sponge for the production of absorption materials and so on. The study presented an effective strategy for preparing wood sponges via using a top-down chemical treatment on low-density balsa wood and paid more attention to the controlling rule of preparation parameters. At the condition that pH of 4.0 (NaClO2 solution), NaOH concentration of 7 wt%, and NaClO2 concentration of 3 wt%, wood sponge with a porosity of 96.47% can be obtained with good resilience and excellent absorption capacity. Excessive concentration of NaOH and NaClO2 will significantly affect the skeletal structure of the wood sponge. After the silylation treatment, the optimal wood sponge was endowed with oil and organic solvents absorption capacity of 2441-17,300 mg g(-1); it can be also recycled by simple extrusion. This highly resilient and recyclable wood sponge with high porosity and oil absorption capacity can be potentially applied for environmental protection.
机译:木材可用于化学处理原位制备木质海绵,可作为污水处理的吸收剂,具有成本低、密度低、孔隙率高、环境友好等优点。以往对木质海绵的研究主要集中在其各种应用上,而对处理条件如NaClO2溶液的pH值和浓度以及NaOH溶液的浓度的影响规律和机理尚未完全了解。这一挑战限制了海绵木材的生产效率和进一步应用于吸附材料的生产等。本研究提出了用自上而下的化学处理方法制备低密度轻木海绵的有效策略,并着重研究了制备参数的控制规律。在pH值为4.0(NaClO2溶液)、NaOH浓度为7%、NaClO2浓度为3%的条件下,可以获得孔隙率为96.47%的木质海绵,具有良好的回弹性和良好的吸附性能。NaOH和NaClO2浓度过高会显著影响木质海绵的骨架结构。经过硅烷化处理后,最佳的木质海绵对油和有机溶剂的吸收能力为2441-17300 mg g(-1);它也可以通过简单的挤压回收。这种高弹性、可回收的木质海绵具有高孔隙率和吸油能力,可用于环境保护。

著录项

  • 来源
    《Journal of Materials Science 》 |2021年第14期| 共18页
  • 作者单位

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

    Guangxi Univ Sch Resources Environm &

    Mat Nanning 530004 Peoples R China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 工程材料学 ;
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号