Hypothesis: Polymer photonic crystals have drawn a lot of interest due to cost-effective fabrication. Although tremendous efforts are tried, almost no large-size photonic crystal (PC) films can be obtained due to different kinds of reasons. The main issues are the tedious process and strict preparation conditions (like high temperature and solvents), sometimes the limitation of the machinery equipment, accordingly they are not conducive to preparation of subsequent large-scale PC films. Hence, there is an urgent desire to develop a technique that can assemble polymer PC films in a large scale at low temperature without solvent.
机译:假设:聚合物光子晶体由于成本效益高而引起了人们的广泛兴趣。尽管人们付出了巨大的努力,但由于各种原因,几乎无法获得大尺寸光子晶体(PC)薄膜。主要问题是繁琐的工艺和严格的制备条件(如高温和溶剂),有时机械设备的限制,因此不利于后续大规模PC薄膜的制备。因此,迫切需要开发一种能够在低温下无溶剂大规模组装聚合物PC膜的技术。

著录项

相似文献

  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号