A foam with high stability for the efficient decontamination of radioactive materials has been prepared by using well-dispersed mesoporous silica nanoparticles (NPs). Three different types of silica NPs were tested: solvent-extracted mesoporous silica (SMS) NPs, calcined mesoporous silica (CMS) NPs, and commercial silica (M-5) NPs. The stability and decontamination efficiency of the foam prepared using SMS NPs was higher than those using other silica NPs. The liquid volume in the foam with the SMS NPs are 10-25 times greater than those containing the CMS and M-5 NPs. The stability of the decontamination foam consisting of SMS NPs is higher because of its higher viscosity; the SMS NPs sample contains a larger number of particles per unit volume and has smaller particle sizes than the CMS and M-5 NPs samples. To investigate the dispersion-agglomeration properties of the silica NPs, the size distributions of the silica NPs in the decontamination foam solutions were determined by using dynamic light scattering. The SMS NPs are smaller than the CMS and M-5 NPs in the decontamination foam solution. For stainless steel 304 and carbon steel specimens corroded with the radionuclide Co-60, decontamination foams containing SMS NPs were found to exhibit a decontamination efficiency 20-40% greater than those of the foams containing the other silica NPs. This superior efficiency arises because the foams prepared with SMS NPs exhibit improved stability and their liquid component can hold larger amounts of the decontamination agent.
机译:通过使用井分散的介孔二氧化硅纳米粒子(NPS)制备具有高稳定性的具有高稳定性的泡沫。测试了三种不同类型的二氧化硅NP:溶剂提取的介孔二氧化硅(SMS)NPS,煅烧的中孔二氧化硅(CMS)NPS和商业二氧化硅(M-5)NPS。使用SMS NPS制备的泡沫的稳定性和去污效率高于使用其他硅NP的泡沫效率。具有SMS NPS的泡沫中的液体体积大于含有CMS和M-5 NPS的液体的10-25倍。由于其较高的粘度,由SMS NPS组成的去污泡沫的稳定性更高; SMS NPS样品包含每个单位体积的大量颗粒,并且具有比CMS和M-5 NPS样品更小的粒度。为了研究二氧化硅NP的分散聚集性,通过使用动态光散射测定脱块泡沫溶液中的二氧化硅NP的尺寸分布。 SMS NPS小于去污泡沫溶液中的CMS和M-5 NPS。对于不锈钢304和碳钢样品,碳钢样品与放射性核素CO-60腐蚀,发现含有SMS NPS的去污泡沫表现出比含有其它硅NPS的泡沫的去污效率为20-40%。这种卓越的效率出现,因为用SMS NPS制备的泡沫表现出改善的稳定性,并且它们的液体成分可以容纳较大量的去污剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号