The chitosan/poly vinyl alcohol membrane was modified by addition of some amine group to the membrane structure utilizing polyethyleneimine (PEI) in order to increase ionic metals adsorbent properties of the membrane. The removal percentage of the modified membranes was compared with the pristine membrane and activated carbon as common adsorbents. The membranes were characterized by FTIR, SEM, swelling degree and porosity measurement. The removal percentage of the membrane containing 0.5 wt.% PEI was more than 60% higher than the activated carbon and more than 40% higher than the pristine membrane. The modified membrane showed excellent adsorption capacity of 112.13, 86.08, and 75.5 mg/g for Cd2+, Cu2+ and Ni2+, respectively at 25 degrees C and pH 6. Adsorption kinetics and equilibrium adsorption isotherm fitted pseudo-second-order kinetic model and Langmuir isotherm model well, respectively. The membrane could be regenerated successfully in Na(2)EDTA aqueous solution with no significant reduction in its adsorption efficiency.
机译:通过将一些胺基加入到膜结构中使用聚乙烯亚胺(PEI)来改变壳聚糖/聚乙烯醇膜,以增加膜的离子金属吸附性。将改性膜的去除百分比与原始膜和活性炭相比,作为常见的吸附剂。膜的特征在于FTIR,SEM,溶胀度和孔隙度测量。含有0.5重量%的膜的去除百分比大于活性炭高出60%,比原始膜高出40%。改性膜分别在25摄氏度和pH6的CD2 +,Cu2 +和Ni2 +的112.13,86.08和75.5mg / g的优异吸附容量为CD2 +,Cu2 +和Ni2 +。吸附动力学和平衡吸附等温线安装伪二阶动力学模型和Langmuir等温线模型良好。可以在Na(2)EDTA水溶液中成功再生膜,其吸附效率没有显着降低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号