Zr2W2P2O15 with larger-negative-thermal-expansion-coefficient (NTEC,-4.01x10(-6) K-1, 143-673 K) is developed by controlling reaction process to avoid the intermediate phase of Zr2WP2O12, whose smaller NTEC limits its application. From 1473 K to1573 K, Zr2WP2O12 forms easily but the reaction between Zr2WP2O12 and WO3 to generate Zr2W2P2O15 is difficult even followed by heating up to 1673 K. However, putting raw materials of ZrO2, WO3 and NH4H2PO4 into a pipe furnace at sintering temperature 1673 K directly, the Zr2W2P2O15 is formed avoiding the intermediate phase of Zr2WP2O12.
机译:通过控制反应过程来开发具有较大阴性热膨胀系数(NTEC,-4.01X10(-6)K-1,143-673k)的Zr2W2P2O15,以避免Zr2WP2O12的中间相,其较小的NTEC限制其应用 。 从1473K至1573 K,Zr2WP2O12易于形成Zr2WP2O12和WO3之间的反应,以产生Zr2W2P2O15,甚至是加热高达1673k的。然而,将ZrO2,WO3和NH4H2PO4的原料置于烧结温度1673k的管道炉中。 直接,形成Zr2W2P2O15避免Zr2WP2O12的中间相。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号