In the field of microelectronics housings made of corundum or sapphire are used, because they resist high mechanical stresses and can be used in extreme environments. For joining these components, sealing materials are necessary, which have a thermal expansion coefficient adapted to corundum or sapphire (8.2x10(-6)K(-1)) and resist high temperature. This can be achieved by glass, which is crystallized during the joining process. However, the temperatures in conventional joining processes are not suitable for the encapsulation of temperature "sensitive components". During a laser joining process only the joining zone is heated up for a short period of time and the components were not destroyed. For this process glasses from the system CaO/MgO/Al2O3/SiO2 were chosen and analyzed with respect to their sintering and crystallization behavior. The glasses could be sintered and crystallized by using the laser joining process. The crystallized glasses have a thermal expansion coefficient between 8.1 x10(-6) K-1 and 9.3 x10(-6) K-1 and hence, show a good match for joining of corundum and sapphire.
机译:在使用刚玉或蓝宝石的微电子壳体领域,因为它们抵抗高机械应力,可用于极端环境。为了加入这些部件,需要密封材料,其具有适应刚玉或蓝宝石(8.2×10(-6)K(-1))并抗蚀于高温的热膨胀系数。这可以通过玻璃实现,该玻璃在加工过程中结晶。然而,常规连接过程中的温度不适用于温度“敏感成分”的封装。在激光连接过程中,仅加热连接区域在短时间内加热,并且部件未被破坏。对于该方法,选择并相对于其烧结和结晶行为来选择并分析并分析CaO / MgO / Al2O3 / SiO 2。通过使用激光连接过程可以烧结并结晶玻璃。结晶玻璃的热膨胀系数在8.1×10(-6)k-1和9.3×10(-6)K-1之间,因此显示出刚玉和蓝宝石的连接很好。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号