Change in Mechanical Properties of Oxide Ceramics by Heat Treatment under Vacuum Condition

机译:真空条件下热处理改变氧化物陶瓷的力学性能

获取原文
获取原文并翻译 | 示例
           

摘要

Alumina and Y_2O_3-partially stabilized zirconia (PSZ) which were typical oxide ceramics were heat-treated in vacuum in holding time of 3h and the temperatures between 1300 deg C and 1600 deg C. All test pieces showed mass loss by the heat-treatment. The amount of mass loss of the alumina was more abounding than that of the Y_2O_3-PSZ. Though the mass loss seemed to he due to vaporization from the sample surface, vapor species did not be identified. Bending strength of alumina and Y_2O_3-PSZ did not show the remarkable change by heat-treatment up to 1500 deg C, hut decreased suddenly at 1600 deg C. It is considered that one of the factors of strength degradation is the grain growth by heat-treatment. In case of the alumina, Vickers hardness showed the decrease of about 10 percent up to 1500 deg C and the decrease of about 30 percent at 1600 deg C. In case of the Y_2O_3-PSZ, Vickers hardness showed the decrease of about 10 percent in all tested temperature range. The degree of degradation of measured physical property of the Y_2O_3-PSZ was smaller than that of the alumina. The Y_2O_3-PSZ was more stable than the alumina for heat treatment.
机译:氧化铝和Y_2O_3-部分稳定的氧化锆(PSZ)在保持时间的保温时间为3小时的真空热处理,并且在1300℃和1600℃之间的温度均受热处理的质量损失。氧化铝的质量损失量比Y_2O_3-PSZ更充分。虽然由于来自样品表面的蒸发而似乎似乎的质量损失,但蒸汽物种未被鉴定。氧化铝和Y_2O_3-PSZ的弯曲强度并未显示出高达1500℃的热处理变化,小屋突然在1600℃下突然下降。认为强度降解的一个因素是通过热量的晶粒生长治疗。在氧化铝的情况下,维氏硬度显示约10%至1500℃的减少,降低约30%,在1600℃下减少约30%。在Y_2O_3-PSZ的情况下,维氏硬度显示约10%的降低所有测试的温度范围。 Y_2O_3-PSZ的测量物理性质的降解程度小于氧化铝。 Y_2O_3-PSZ比用于热处理的氧化铝更稳定。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号