Effect of bamboo leaf ash on cement stabilization of Makurdi shale for use as flexible pavement construction material

机译:竹灰对柔性路面建筑材料Makurdi页岩水泥稳定的影响

获取原文
获取原文并翻译 | 示例
       

摘要

A study was carried out on the cement stabilization of Makurdi shale treated with bamboo leaf ash (BLA), for use as flexible pavement construction material. Classification, Compaction, Consistency, California Bearing Ratio (CBR) and unconfined compressive strength (UCS) tests, were conducted on Makurdi shale specimen treated with Cement and BLA in combined incremental order of 2 % up to 14 % cement, and 4 % up to 20 % BLA of dry weight of soil sample respectively. Results of tests showed that Makurdi shale can be classified as an A-7-6, CH and high swell potential soil by the AASHTO, USCS and NBRRI classification systems respectively. The plasticity index (PI) reduced from 39.4 % for untreated Makurdi shale to 4.7 % at 14 % cement + 20 % BLA. Maximum dry density (MDD) of untreated shale increased from 1.49 Mg/m~3 to a peak value of 1.80 Mg/m~3 at 0 % BLA + 14 % cement. While, the optimum moisture content (OMC) of shale increased from 14.5 % to 33.1 % at 14 % Cement + 20 % BLA. Maximum soaked CBR and 7 day UCS values of 80 % and 1783.9 kN/m~2 was obtained at 14 % Cement + 20 % BLA. Based on the results of the different tests, the use of Makurdi shale treated with 14 % cement + 20 % BLA are recommended for use as sub-base materials in flexible pavement.
机译:对用竹叶灰(BLA)处理的Makurdi页岩的水泥稳定性进行了研究,以用作柔性路面建筑材料。对用水泥和BLA处理的Makurdi页岩样品进行了分类,压实,稠度,加利福尼亚承载比(CBR)和无侧限抗压强度(UCS)试验,组合增量顺序为2%至14%水泥和4%至土壤样品干重的BLA分别为20%。测试结果表明,Makurdi页岩可分别通过AASHTO,USCS和NBRRI分类系统分类为A-7-6,CH和高溶胀潜力土壤。塑性指数(PI)从未处理的Makurdi页岩的39.4%降至14%水泥+ 20%BLA时的4.7%。未处理的页岩的最大干密度(MDD)从1.49 Mg / m〜3增加到在0%BLA + 14%水泥下的峰值1.80 Mg / m〜3。同时,在14%水泥+ 20%BLA的情况下,页岩的最佳含水量(OMC)从14.5%增加到33.1%。在14%水泥+ 20%BLA的情况下,获得的最大浸泡CBR和7天UCS值为80%和1783.9 kN / m〜2。根据不同测试的结果,建议使用经过14%水泥+ 20%BLA处理的Makurdi页岩作为柔性路面的基础材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号