A simple metallurgical process for fabricating vertical oxide nano-rod array structures with internal oxidation of alloys is described. Oxidation at high-temperatures and under low oxygen partial pressures can develop internally rod-like oxide precipitates in some dilute alloys such as Ni(Al) solid solutions. The vertical oxide nano-rod arrays can be developed on the metal substrates or components by removing the metallic matrix of the internal oxidation zone. Al _2O _3 or NiAl _2O _4 spinel nano-rod arrays were prepared by using M(Al) solid solutions. Pack cementation process to develop Ni(Al) solid solution zone on a metal surface was used for the fabrication of vertical nano-rod arrays on Ni substrates with desired shape. Near-net shape Ni substrates with vertical oxide nano-rod array structures on their surfaces can be prepared by using pack cementation and internal oxidation. Fabrication of vertical nano-rod arrays with Co(Al) and Fe(Al) solid solutions were also described briefly.
机译:描述了一种利用合金内部氧化制造垂直氧化物纳米棒阵列结构的简单冶金工艺。在高温和低氧分压下的氧化会在某些稀合金(例如Ni(Al)固溶体)中内部形成棒状氧化物沉淀。垂直氧化物纳米棒阵列可通过去除内部氧化区的金属基质而在金属基底或部件上显影。通过使用M(Al)固溶体制备Al _2O _3或NiAl _2O _4尖晶石纳米棒阵列。在金属表面上形成Ni(Al)固溶区的填充胶结工艺用于在具有所需形状的Ni基板上制造垂直纳米棒阵列。可以通过使用填充胶结和内部氧化来制备在其表面上具有垂直氧化物纳米棒阵列结构的近最终形状的Ni衬底。还简要介绍了用Co(Al)和Fe(Al)固溶体制备垂直纳米棒阵列的过程。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号