A dyeing machine part made of type 304 stainless steel was severely attacked in contact with 0 1 mol/l sulfamic acid (amidosulfuric acid, H_2NSO_3H) solution of pH 1.2 contaminated with hydrosulfito (Na_2S_2O_4) at 60 deg C. This study was conducted at 30 deg C and succeeded to reproduce the enhanced attack with corrosion rates up to 5.4 mm per year under added Na_2S_2O_4 concentrations between 0.1 and 5 mmol/l at pHs lower than 2.2. The steel dissolved at active potentials with deposition of black corrosion products and generation of H_2S gas on its surface. Such high rates of corrosion was attributed to the effects of Na_2S_2O_4 which increased both anodic dissolution of the steel and cathodic current for reduction of S~0 to H_2S. When the Na_2 S_2O_4 concentration increased over 7 mmol/l, the increased cathodic current passivated the steel by exceeding the anodic one which was inhibited by protective surface film consisting mainly of S~0 and NiS.
机译:由304型不锈钢制成的染色机部件遭到60℃的含有Hydrosulfito(Na_2S_2O_4)的pH 1.2的pH 1.2接触的接触被严重攻击。该研究在30时进行了这项研究 DEG C并成功地再现增强率,在添加Na_2S_2O_4浓度下在低于2.2的pHS之间的Na_2S_2O_4浓度下,每年腐蚀速率可达5.4毫米。 钢溶解在具有黑色腐蚀产物的积极电位上,并在其表面上产生H_2S气体。 这种高腐蚀率归因于NA_2S_2O_4的效果,其增加了钢的阳极溶解和阴极溶解,以降低S〜0至H_2S。 当Na_2 S_2O_4浓度超过7mmol / L时,通过超过主要由S〜0和NIS构成的保护表面膜抑制的阳极氧化物,增加的阴极电流钝化了钢。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号