首页> 外文期刊>Journal of the European Ceramic Society >A novel Co-ions complexation method to synthesize pyrochlore La(2)Zr(2)O7
【24h】

A novel Co-ions complexation method to synthesize pyrochlore La(2)Zr(2)O7

机译:一种新的共离子络合方法,合成纤维晶叶(2)ZR(2)O7

获取原文
获取原文并翻译 | 示例

摘要

Pure pyrochlore Lanthanum zirconate (LZ) was synthesized by co-ions complexation method (CCM) at 1300 degrees C, which is 300 degrees C lower than that by solid-state method (SSM). At 1450 degrees C, the 12 prepared by CCM possessed lower thermal conductivity (1.15 W/m K) than that obtained by SSM (1.99 W/m K). This significant decrease may be caused by the different grain size, which is 300 nm and 2.5 mu m synthesized by CCM and SSM, respectively. 12 precursor was belt-shaped and the belt shorten and the grain grown with the temperature increasing. Fourier transform infrared spectroscopy suggested the solidification in CCM forms from the complexation between La3+, Zr4+ and (CHCOO-)-C-3, which is the key for solidification. Compared to SSM, CCM is a lower temperature and simpler technology to synthesize nano-size 12 and other rare-earth oxides.(C) 2017 Elsevier Ltd. All rights reserved.
机译:通过共离子络合方法(CCM)在1300℃下合成纯烧火镧锆锆(LZ),其是通过固态方法(SSM)低300℃。 在1450℃下,通过CCM制备的12具有较低的导热率(1.15W / M K),比SSM(1.99W / M K)所获得的。 这种显着的降低可能是由CCM和SSM合成300nm和2.5μm的不同粒度引起的。 12个前体是带形的,皮带缩短和随温度升高而生长的晶粒。 傅里叶变换红外光谱表明,从La3 +,Zr4 +和(Chcoo - ) - C-3之间的络合中的CCM形式凝固,这是凝固的关键。 与SSM相比,CCM是较低的温度和更简单的技术,用于合成纳米尺寸12和其他稀土氧化物。(c)2017 Elsevier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号