Certain materials such as wax, when incorporated into rubber formulations, bloom and form a surface barrier layer against ozone attack. The ozone resisting film results in an unpleasant appearance on the rubber surface. In tyres, sidewalls are more susceptible to ozone attack leading to degradation both in dynamic and static conditions. Also, tyre appearance is an important factor in quality control visual inspections and the acceptance of the final product in the market. In this paper, the effect of oil contents in different waxes on the physico-mechanical properties of rubber vulcanisates was investigated. It was found that in UV-Vis spectra, at different ageing times, the absorbance of extracted cured tyre sidewall compound samples at 472 nm showed the concentration of the antidegradants in the rubber vulcanisates. The migration, based on protecting function leading to degrading the antidegradants after the ageing time of 72 h. With 72 h of ageing time in the ozone chamber, the waxes with higher oil content showed a faster migration of antidegradants to the surface of the rubber vulcanisates and degraded faster than the waxes with lower oil content.
机译:当掺入橡胶制剂中时,诸如蜡的某些材料,绽放并形成抗臭氧侵蚀的表面阻挡层。臭氧抗蚀剂导致橡胶表面上的令人不愉快的外观。在轮胎中,侧壁更容易受到臭氧攻击的影响,导致动态和静态条件下降。此外,轮胎外观是质量控制视觉检查的重要因素和市场上最终产品的验收。本文研究了不同蜡对不同蜡对橡胶硫化酸盐物理机械性能的影响。发现在不同老化时间的UV-Vis光谱中,在不同的老化时间,在472nm处的提取的固化轮胎侧壁化合物样品的吸光度显示橡胶硫化酸盐中的抗生素的浓度。迁移,基于保护功能,导致在72小时的老化时间后降解抗灭菌剂。在臭氧室中具有72小时的老化时间,具有更高油状物的蜡显示出抗橡胶硫化物表面的抗灭弧剂的迁移得更快,并且比具有较低含油含量的蜡更快地降解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号