New method of measuring water permeability of adhesive resin films.

机译:测量粘合树脂薄膜透水性的新方法。

获取原文
获取原文并翻译 | 示例
       

摘要

PURPOSE: To adapt a simple gravimetric method to measuring the permeability of adhesive resin films to liquid water, and to compare this to the water vapor permeability of the same resins. METHODS: Using commercially-available permeability cups designed for industrial permeability testing, the loss of mass of water vapor or liquid water from a stainless steel cup sealed with a resin film was measured over 1-2 days. The permeabilities of Parafilm (control), Clearfil SE Bond adhesive, Xeno IV and One-Up Bond F were compared. RESULTS: The lowest resin film permeability was obtained with Clearfil SE Bond adhesive films. The permeabilities ofXeno IV and One-Up Bond F to liquid water were 2.76 and 3.27-fold higher (P < 0.001) than that of Clearfil SE Bond adhesive. Liquid water permeability was always 2.8-3.8-fold higher (P < 0.05) than water vapor transmission rate. It was concluded that quantitative comparisons of the permeability properties of resin films can be made gravimetrically. The large permeability cups that are available commercially may be reduced in size in the future for measuring dentin adhesive films with smaller surface areas that are less liable to contain imperfections.
机译:目的:采用一种简单的重量分析法来测量粘性树脂膜对液态水的渗透率,并将其与相同树脂的水蒸气渗透率进行比较。方法:使用专为工业渗透性测试而设计的市售渗透性杯,在1-2天内测量了用树脂膜密封的不锈钢杯中水蒸气或液态水的质量损失。比较了Parafilm(对照),Clearfil SE Bond粘合剂,Xeno IV和One-up Bond F的渗透性。结果:使用Clearfil SE Bond粘合膜获得了最低的树脂膜渗透性。 Xeno IV和One-up Bond F在液态水中的渗透率比Clearfil SE Bond粘合剂高2.76倍和3.27倍(P <0.001)。液体的水渗透率始终比水蒸气透过率高2.8-3.8倍(P <0.05)。结论是可以通过重量分析法定量比较树脂薄膜的渗透性。将来可减小可商购的大渗透性杯的尺寸,以用于测量表面积较小,不易包含瑕疵的牙本质粘合膜。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号