This study presents the recovery of oxide-carbonate lead-zinc ores using different chemical reagents under different test conditions by flotation. The run-of-mine oxide-carbonate Pb-Zn ore contains 9.05% Pb and 11.97% Zn with a major mineralization of smithsonite and cerussite. First experimental work was grinding tests to reduce -106 urn size fractions with two 15-minute grinding stages. Pre-flotation tests gave similar results for Pb, but neither pH, ZnSO_4, CuSO_4 nor collectors like AERO 3477, 3501 and 8651 made favorable effect on the recovery of Zn. Therefore, the studies were emphasized for recovering Pb concentrate by changing the amount of chemicals used, such as CMC, Na_2S, AERO promotor. After six stage of flotation with 350 g/t KAX, 275 g/t AERO 407, 7500 g/t Na_2S, 1000 g/t CMC, the concentration of 70.93% Pb with 71.56% recovery was achieved. The 91.51% Zinc remained in the tailing with 14.66% Zn grade.
机译:本研究通过浮选在不同的试验条件下使用不同的化学试剂呈现氧化物 - 碳酸铅锌矿矿石的恢复。 含铅流动的氧化物 - 碳酸盐Pb-Zn Ore含有9.05%Pb和11.97%Zn,具有史密松矿床和Cerussite的主要矿化。 第一个实验工作是磨削测试,以减少2106个瓮尺寸分数,具有两个15分钟的研磨阶段。 预浮选测试对Pb进行了类似的结果,但PH,ZnSO_4,CUSO_4也不是Aero 3477,3501和8651等收集器对Zn的回收作出了有利影响。 因此,强调研究通过改变所用的化学物质,例如CMC,NA_2S,Aero促进剂来回收PB浓缩物。 在用350g / t kax的浮选六个阶段,275g / t航空407,7500g / t na_2s,1000g / t cmc,浓度为70.93%的浓度,达到71.56%回收率。 91.51%的锌留在尾矿中,Zn等级为14.66%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号