PROPERTIES OF MEDIUM-DENSITY FIBREBOARDS BONDED WITH DEXTRIN-BASED WOOD ADHESIVE

机译:用糊精木粘合剂粘合中密度纤维板的性质

获取原文
获取原文并翻译 | 示例
           

摘要

This study focuses on manufacturing of medium density fibreboard (MDF) panels bonded with dextrin-based wood adhesive and crosslinked in situ with various weight ratios of synthetic (e.g., polymeric-methane diphenyl-diisocyanate, pMDI) or bio-based (e.g., glyoxal) crosslinkers. The physical and mechanical properties of the panels were evaluated and compared with those from panels without crosslinker (control). Modulus of rupture (MOR) and internal bond (IB) strength of the MDF panels were considerably increased by increasing the crosslinkers' content. While, slight improvements were observed in modulus of elasticity (MOE) of the panels as a function of crosslinker type and content. Addition of crosslinkers clearly reduced the thickness swelling (TS) and water absorption (WA) of the panels, whereas, the panels with pMDI showed superior performances than the control and glyoxal added ones within 4 h and 24 h immersion in water. The results indicate the potential of dextrin as wood panel adhesive along with the use of appropriate crosslinkers.
机译:该研究侧重于制造与基于糊精的木材粘合剂的中密度纤维板(MDF)面板,并以原位与合成的合成(例如,聚合物 - 甲烷二苯基 - 二异氰酸酯,PMDI)或生物基(例如,乙二酰基)交叉链接者。评估面板的物理和力学性能,并与没有交联剂(对照)的面板的物理和机械性能。通过增加交联剂的含量,MDF面板的破裂模量(MOR)和内键(IB)强度大大增加。虽然,作为交联剂类型和含量的函数,在面板的弹性模量(MOE)模量中观察到轻微改善。交联剂的添加显然降低了面板的厚度膨胀(TS)和吸水(WA),而具有PMDI的面板显示出优于4小时内的对照和乙二醛添加的表现优异的表现和24小时浸入水中。结果表明糊精作为木板粘合剂以及使用适当的交联剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号