In order to reflect the ability of comprehensive dealkalization and desulfurization of BF slag more accurately, the K~(2)S capacity was proposed. The effects of w (CaO)/ w (SiO~(2)), w (MgO) and w (Al~(2)O~(3)) on the ability of comprehensive dealkalization and desulfurization were studied at 1773?K using gas-slag equilibrium techniques. The results showed that with an increase of w (CaO)/ w (SiO~(2)), the comprehensive desulfurization and dealkalization capacity of BF slag increases firstly and then decreases. When w (CaO)/ w (SiO~(2)) is 1.0, the $${ext{C}}_{{{ext{K}}_{ 2} {ext{S}}}}$$ C K 2 S reaches the maximum value. As w (MgO) increases with w (CaO)/ w (SiO~(2)) constant, the $${ext{C}}_{{{ext{K}}_{ 2} {ext{S}}}}$$ C K 2 S of BF slag increases firstly and then decreases. When w (MgO) is 10.58%, the $${ext{C}}_{{{ext{K}}_{ 2} {ext{S}}}}$$ C K 2 S reaches the maximum value. As w (MgO) increases with [ w (CaO)?+? w (MgO)]/ w (SiO~(2)) constant, the $${ext{C}}_{{{ext{K}}_{ 2} {ext{S}}}}$$ C K 2 S of BF slag decreases. The use of MgO instead of CaO can deteriorate the comprehensive desulfurization and dealkalization capacity. With an increase of w (Al~(2)O~(3)), the $${ext{C}}_{{{ext{K}}_{ 2} {ext{S}}}}$$ C K 2 S of BF slag increases firstly and then decreases. When w (Al~(2)O~(3)) is 15.1%, the $${ext{C}}_{{{ext{K}}_{ 2} {ext{S}}}}$$ C K 2 S reaches the maximum value. It is suggested that w (CaO)/ w (SiO~(2)) remains at about 1.0 in blast furnace production, w (MgO) is maintained at about 10.58%, and w (Al~(2)O~(3)) is maintained at about 15.1%.
机译:为了更准确地反映BF渣的全面探索和脱硫能力,提出了K〜(2)的容量。 W(CaO)/ W(SiO〜(2)),W(MgO)和W(Al〜(2)O〜(3))对综合销售和脱硫能力的影响进行了1773 k气渣均衡技术。结果表明,随着W(CAO)/ W的增加(SiO〜(2)),BF渣的综合脱硫和拒绝能力首先增加,然后减少。当w(cao)/ w(siO〜(2))为1.0时,$$ { text {c}} _ {{{ text {k}} _ {2} { text {s}}}} $$ CK 2 S达到最大值。随着W(MgO)随W(CAO)/ W(SIO〜(2))常数增加,$$ { text {c}} _ {{{ text {k}} _ {2} { text { S}}} QF渣的$$ CK 2 S首先增加,然后减少。当W(MgO)为10.58%时,$$ { text {c}} _ {{{ text {k}} _ {2} { text {s}}} $$ ck 2 s达到最大值价值。随着W(MgO)随[W(CAO)吗?+? W(MgO)] / W(SIO〜(2))常数,$$ { text {c}} _ {{ text {k}} _ {2} { text {s}}} $ BF渣的$ CK 2 S降低。使用MgO代替CAO可以恶化综合脱硫和销售能力。随着W的增加(Al〜(2)O〜(3)),$$ { text {c}} _ {{{ text {k}} _ {2} { text {s}}} BF渣的$$ CK 2 S首先增加,然后减少。当W(2)O〜(3))为15.1%时,$$ { text {c}} _ {{{ text {k}} _ {2} { text {s}}} $$ CK 2 S达到最大值。建议W(CaO)/ W(SiO〜(2))保持在高炉生产中约1.0,W(MgO)保持在约10.58%,而W(Al〜(2)O〜(3)中保持)保持在约15.1%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号