首页> 外文期刊>Transactions of the Indian Institute of Metals >The Analysis of Low Temperature Toughness on X80 Pipeline Steel Welded Joint
【24h】

The Analysis of Low Temperature Toughness on X80 Pipeline Steel Welded Joint

机译:X80管道钢焊接接头低温韧性分析

获取原文
获取原文并翻译 | 示例
           

摘要

Aiming at the security problems of pipeline steel application, the different positions of the welded joints of circumferentially welding pipeline of X80 steel were investigated by microstructure observation, the hardness, Charpy impact toughness and crack tip opening displacement (CTOD) test at low temperature. The Vickers hardness test results show that there are local softened regions in heat-affected zone (HAZ). Charpy impact test indicate that the ductile-brittle transition temperature of weld is below -60 degrees C, the ductile-brittle transition temperature of HAZ is around -38 degrees C. CTOD test reveal that the fracture toughness of HAZ shows a large fluctuation since it is in the ductile-brittle transition temperature regime.
机译:针对管道钢应用的安全问题,通过微观结构观察,低温下的微结构观察,硬度,夏比冲击韧性和裂纹尖端打开位移(CTOD)测试来研究X80钢的圆周焊接管道的焊接接头的不同位置。 维克斯硬度测试结果表明,热影响区域(HAZ)中存在局部软化区域。 夏比冲击试验表明,焊缝的韧性脆性转变温度低于-60℃,危险的韧性 - 脆性转变温度约为-38℃。CTOD试验表明,HAZ的断裂韧性显示出自IT以来的大幅波动 处于韧性脆性过渡温度制度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号