Objective: To compare the clinical performance of two glass-ionomer cements in combination with two light-cured coatings in Class II cavities. Method and materials: In total, 43 Equia Fil/Equia Coat and 42 Fuji IX GP Fast/Fuji Coat LC restorations were placed, in 34 patients. Only Class II cavities with two-or three-surface restorations were included. The clinical performance was evaluated at baseline, after 1, 2, and 3 years using the FDI criteria. For the statistical analysis, Fisher exact test, Wilcoxon signed-rank test and Mann-Whitney U test were applied. The success and survival of the restorations were calculated with the Kaplan-Meier method and a log-rank test was used to detect significant differences between the tested materials. Results: At the 3-year recall, no significant differences could be detected between the two glass-ionomer cements for any of the evaluated criteria (Mann-Whitney U test, P> .05). When comparing the baseline with the recall data at 3 years for each material separately, significant changes could be observed in both materials for the criteria "surface luster," "fracture of material and retention," and "approximal anatomical form" (Wilcoxon signed-rank test, P < .05). Additionally, the Equia Fil restorations showed a notable change for the criteria "marginal adaptation" (Wilcoxon signed-rank test, P= .039). At the 3-year follow up, the Equia Fil and the Fuji IX GP Fast restorations exhibited an overall survival rate of 86.21% and 84.0%, respectively. Conclusion: The two glass-ionomer cements tested performed similarly in Class II cavities in adult patients, with a moderate to high failure rate after 3 years.
机译:目的:比较两种玻璃离聚物水泥与II类腔内两种光固化涂料的临床性能。方法和材料:总共43架欧洲港/欧洲外套和42例富士IX GP Fast / Fuji Coat LC修复,34名患者。仅包括具有两个或三表面修复物的II类空腔。使用FDI标准,在1,2和3年之后评估临床表现。对于统计分析,渔业精确试验,威尔科逊签名级别测试和Mann-Whitney U测试。用Kaplan-Meier方法计算修复的成功和生存率,使用日志秩检测来检测测试材料之间的显着差异。结果:在3年的召回中,对于任何评估标准(Mann-Whitney U测试,P> 0.05)之间的两个玻璃离聚物水泥之间没有检测到显着差异。当将基线与召回数据分别3年进行比较时,可以在标准“表面光泽”的标准中可以观察到显着的变化“材料和保留的裂缝”和“近似解剖学”(Wilcoxon签名 - 等级测试,p <.05)。此外,Equia FIL修复结果显示了标准“边际适应”(Wilcoxon签名 - 秩测试,P = .039)的显着变化。在3年的跟进后,Equia Fil和Fuji IX GP快速修复分别显示出86.21%和84.0%的总生存率。结论:在成人患者的II类腔内测试的两种玻璃离聚物水泥在成人患者的II类腔中进行,3年后具有中度至高的失效率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号