In the present work, sandwich hybrid composites have been fabricated using hand layup technique followed by compression molding process. Glass and basalt fabrics were used with epoxy resin to fabricate the sandwich composites. The fabrics were used in both untreated and treated conditions using hydrochloric acid and sodium hydroxide solutions. The Fourier transform infrared study conducted on the fabrics before and after the surface treatment shows the effectual impregnation of acid and base on the fabric by the formation of ions on the surfaces. The tensile and hardness tests were conducted as per the ASTM D638-10 and ASTM D2240 standards. The results show that hybridization and surface treatment improve tensile strength and hardness in all the composites. In particular, the hydrochloric acid-treated sandwich composites with basalt fabric as core and glass fabric as skin have recorded the highest tensile strength of 356.39 MPa. The experimental values have been validated using the simulation results of finite element analysis in ANSYS 15.0 with a minimum deviation of 0.47%.
机译:在本作工作中,使用手动叠层技术进行了夹层混合复合材料,然后用压缩成型方法制造。玻璃和玄武岩织物与环氧树脂一起使用以制造夹层复合材料。使用盐酸和氢氧化钠溶液在未处理和处理的病症中使用织物。在表面处理之前和之后在织物上进行的傅里叶变换红外研究表明,通过在表面上形成离子,在织物上的有效浸渍和基础。根据ASTM D638-10和ASTM D2240标准进行拉伸和硬度试验。结果表明,杂交和表面处理在所有复合材料中提高拉伸强度和硬度。特别是,作为核心和玻璃织物的盐酸处理的夹心复合材料作为皮肤的核心和玻璃织物已经记录了356.39MPa的最高拉伸强度。使用ANSYS 15.0中有限元分析的仿真结果进行了验证了实验值,最小偏差为0.47%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号