摘要

The curing behavior and microstructure of natural rubber/silica foams were studied. Error function-based and autocatalytic models were correlated with the curing characteristics data of samples. The incorporation of silica into natural rubber caused an increase in the foam density and decrease in the cell size. Moreover, by increasing the curing temperature, cell size became larger and cell size distribution became non-uniform. It was thought that the higher temperature of foaming limited the bubble growth due to faster curing reaction. Lower viscosity and lower strength of rubber at high temperature increased the cell coalescence resulting in larger cell size and non-uniform cell distribution.
机译:研究了天然橡胶/二氧化硅泡沫的固化行为和微观结构。 基于误差函数和自催化模型与样品的固化特性数据相关。 将二氧化硅掺入天然橡胶引起泡沫密度的增加并降低细胞尺寸。 此外,通过增加固化温度,电池尺寸变得更大,细胞尺寸分布变得不均匀。 据认为,发泡的较高温度限制了由于更快的固化反应引起的泡沫增长。 橡胶在高温下较低的粘度和较低强度增加了细胞聚结,导致细胞尺寸较大和不均匀的细胞分布。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号