首页> 外文期刊>Oriental Journal of Chemistry: An International Research Journal of Pure & Applied Chemistry >The Preparation of Nano-oxides of Zinc and Barium of [Ba (o-phen)4] [Zn (EDTA)], [Zn(o-phen)4]2 [ Ba(SCN)6], and Synthesis of ZrO2 Nanoparticles by Chemical Methods
【24h】

The Preparation of Nano-oxides of Zinc and Barium of [Ba (o-phen)4] [Zn (EDTA)], [Zn(o-phen)4]2 [ Ba(SCN)6], and Synthesis of ZrO2 Nanoparticles by Chemical Methods

机译:锌的纳米氧化物和[BA(O-Phen)4] [Zn(EDTA)],[Zn(O-Phen)4] 2 [Ba(SCN)6]的制备,以及ZrO2纳米颗粒的合成 通过化学方法

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

For the preparation of Nano-oxides of Zinc and Barium, first, the two-component complexes [Ba(o-phen)4] [Zn (EDTA)], [Zn(o-phen)4]2 [Ba(SCN)6] were produced, then they were heated for one hour in 700 and 800 °C inside the electrical furnacet. The complexes have been characterized by elemental analysis, FT-IR. To Synthesize nano-metric ZrO2, the chemical method was used, which was the most economical method. The minimum temperature for performing alkaline fusion using NaOH and KOH catalysts - with the ratio of twice the weight of Zirconium silicate as the optimum flux - was determined to be 850 °C. Under optimum conditions, Zirconia powders were synthesized in 900 °C with longetitivty of two hours.Using X-ray diffraction (XRD) and scanning electron microscopy (SEM), the Nanometric state of particles of Zirconium oxide, Barium, and Zinc oxide was confirmed.
机译:为了制备锌和钡的纳米氧化物,首先,双组分络合物[Ba(O-Pen)4] [Zn(EDTA)],[Zn(O-Phen)4] 2 [Ba(SCN) 制成6],然后将它们在700和800°C内加热1小时,电热带。 复合物的特征在于元素分析,FT-IR。 为了合成纳米公式ZrO2,使用化学方法,这是最经济的方法。 使用NaOH和KOH催化剂进行碱性融合的最小温度 - 用锆硅酸锆重量的比例为最佳助焊剂的比例为850℃。 在最佳条件下,氧化锆粉末在900℃下合成,长度为2小时。X射线衍射(XRD)和扫描电子显微镜(SEM),确认氧化锆颗粒颗粒颗粒颗粒 。