INVESTIGATION OF MECHANICAL, THERMAL, AND MORPHOLOGICAL PROPERTIES OF EPDM COMPOUNDS CONTAINING RECLAIMED RUBBER

机译:EPDM化合物的机械,热和形态学性能研究含有再生橡胶的方法

获取原文
获取原文并翻译 | 示例
           

摘要

The disposal of polymeric and hazardous materials is an important global issue. Thus, the mechanochemical reclaiming of waste EPD Mrubber was carried out using disulfide oil (DSO), oily waste produced in gas refineries, as a reclaiming agent at a specific operation condition. Reclaimed rubber was characterized by crosslink density, sol-gel, and Mooney viscosity measurements. Following the study, blending of different portions of reclaimed rubber (20, 40, 60, and 80 wt%) with virgin EPD Mrubber was carried out. Results showed that the addition of 60wt% of reclaimed rubber to the virgin EPD Mrubber had no adverse effect on the scorch and optimum curing time. Also, mechanical properties of revulcanized rubber improved when 40 wt% of virgin EPDM rubber was replaced with the reclaimed rubber. Scanning electron microscope and thermal gravimetric analyses of the samples revealed the effect of addition of reclaimed rubber on the rubber matrix and thermal stability of revulcanized samples, respectively. This study proposes a new route for solving the problem of disposal of the waste materials.
机译:聚合物和危险物质的处置是一个重要的全球问题。因此,使用二硫化物油(DSO),在气体炼油厂中产生的油性废物,作为特定操作条件的回收剂进行的机制回收。通过交联密度,溶胶和门尼粘度测量表征回收橡胶。在研究之后,进行与原始EPD MRUBBER的再生橡胶(20,40,60和80wt%)的不同部分的混合。结果表明,在维京EPD MRBOBBER中加入60wt%的再生橡胶对烧焦和最佳固化时间没有不利影响。此外,当用再生橡胶替换40重量%的维珍EPDM橡胶时,逆升压橡胶的机械性能提高。扫描电子显微镜和样品的热重分析显示了在橡胶基质上添加了再生橡胶的效果,分别对逆脉冲样品的热稳定性。本研究提出了一种解决废料处理问题的新路线。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号