Bi-loaded plastic scintillators were successfully synthesized using the solvent evaporation method and were used as detectors for synchrotron X-ray radiation. The photoluminescence emission spectra and X-ray-excited radio-luminescence spectra of all prepared plastic scintillators presented broad emission bands in the range of 350-500 nm, which derived from the fluorescence of the organic phosphor, 2-(4-tert-butylphenyl)-5-(4 biphe nylyl)-1,3,4-oxadiazole. The detection efficiency of 1 mm thick plastic scintillators for high-energy X-ray photons was increased by the addition of Bi compounds (up to 2.3 wt%) and reached 67% of that of EJ-256, the commercially available Pb 5 wt% loaded plastic scintillator. Subnanosecond time resolution was successfully achieved for all scintillators.
机译:使用溶剂蒸发方法成功合成了双装塑料闪烁体,用作同步X射线辐射的探测器。 所有制备的塑料闪烁体的光致发光发射光谱和X射线激发无线电光谱呈现在350-500nm的范围内的宽发射带,其衍生自有机磷光体的荧光,2-(4-叔丁基苯基 )-5-(4个Biphe Nylyl)-1,3,4-氧代唑。 通过添加BI化合物(高达2.3wt%)增加1mm厚的塑料闪烁剂的检测效率,并达到EJ-256的67%,可商购的PB 5wt% 装载塑料闪烁体。 所有闪烁器都成功实现了亚纳十四秒的时间分辨率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号